he finishing cotton fabric treated with different mixture ratio of nano particles TiO2and sodium hypophosphite monohydrate catalyst and curing with the crosslinking agent liquid MA/CA is 75/25 and the treated concentration is 8%.The effects of temperature and time of curing and the concentration of TiO2,sodium hypophosphite monohydrate and additive TEA on wrinkle recovery angle value and physical properties of treated fabrics were extensively studied .Based on the experimental results,the wrinkle recovery angle ,graft percentage and effect of graft percentage increased with cured temperature and time ,but strength and whiteness are appositive,Used mixture catalyst cade the wrinkle recovery angle and strength rise up ,but whiteness and softness are appositive .The whiteness and strength increased with used additive TEA,but the wrinkle recovery angle went down .lBased on the experimenta results ,the wrinkle recovery angle ,graft percentage and effect of graft percentage increased with curde temperature and time ,but strength and whiteness are appositive .Used mixture catayst made the wrinkle recovery angle and strength rise us, but whiteness and softeness are appositive. The whiteness and strength increased with used additive TEA ,but the wrinkle recovery angle went down .